Elastomers, frozen foods, cryoprotectants and battery electrolytes all show their key transitions well below room temperature. With liquid nitrogen this DSC reaches −180 °C; a mechanical cooler covers −90 to 600 °C without consumables. Liquid nitrogen use is about 1–3 L per hour. A positive-pressure dry gas purge prevents ice forming on the cell during long runs.

Temperature range
−180–600 °C (liquid nitrogen)
Mechanical cooling range
−90–600 °C
Heating rate
0.1–50 °C/min
Cooling rate
up to 30 °C/min (mechanical)
Temperature accuracy
±0.1 °C
Inquiry Now

Packing & Shipping

Place of originChina (dispatched from Shanghai)
BrandLiquid International / OEM on request
Export packingFumigation-free plywood case or reinforced carton
Loading portShanghai / Ningbo (others on request)
Payment termsT/T, L/C at sight (confirmed on quotation)
Trade termsEXW, FOB, CFR, CIF, DAP

Typical export terms — final terms are confirmed on the proforma invoice.

Product Description 产品描述

Elastomers, frozen foods, cryoprotectants and battery electrolytes all show their key transitions well below room temperature. With liquid nitrogen this DSC reaches −180 °C; a mechanical cooler covers −90 to 600 °C without consumables. Liquid nitrogen use is about 1–3 L per hour. A positive-pressure dry gas purge prevents ice forming on the cell during long runs.

Highlights

  • Two cooling routes: liquid nitrogen to −180 °C or mechanical to −90 °C
  • Mechanical cooling rate up to 30 °C/min
  • Positive-pressure dry purge keeps the cell frost-free
  • ±0.02 °C precision for subtle low-temperature transitions

Applications

  • Elastomer and adhesive glass transitions
  • Frozen food and ice behaviour
  • Fat crystallization studies
  • Biologic and cryoprotectant characterisation
  • Battery electrolyte low-temperature behaviour

Specifications 技术参数

ParameterValue
Temperature range 温度范围 −180–600 °C (liquid nitrogen)
Mechanical cooling range 机械制冷范围 −90–600 °C
Heating rate 升温速率 0.1–50 °C/min
Cooling rate 降温速率 up to 30 °C/min (mechanical)
Temperature accuracy 温度准确度 ±0.1 °C
Temperature precision 温度重复性 ±0.02 °C
Coolant consumption 冷却剂消耗 1–3 L liquid nitrogen per hour
Anti-icing 防结霜方式 Dry-gas purge with positive pressure
Sample mass 样品质量 2–20 mg
Calibration standards 校准标准 Indium, cyclohexane, water
Model No.DSC-0005
Place of originChina (dispatched from Shanghai)

Applicable standards 适用标准

ASTM E967 ASTM E968 ASTM E1356 ASTM E1269 ISO 11357-1 ISO 11357-2 USP <891>

Chinese national standards (GB/T, JJG) and international standards referenced for this product type. Test reports and certificates are supplied with the quotation on request.

Packing & Shipping 包装与运输

Export packing

Fumigation-free plywood case or reinforced carton

Every unit is power-tested before packing; enclosed in shock foam and moisture barrier; wooden cases comply with ISPM 15.

Loading port

Shanghai / Ningbo (others on request)

Full container load (FCL), less-than-container load (LCL) or air freight; complete export documentation provided.

Inquiry Now 索取报价

Complete the form below — an export engineer will send technical configurations and a formal proforma invoice within 24 hours.

Products in this inquiry: Low-Temperature Differential Scanning Calorimeter (DSC-0005)

We reply within 24 hours (Beijing Time, UTC+8). Your details are used only to answer this inquiry.

Related products

5 models

Send your equipment list — receive a formal quotation within 24 hours

Single instruments, complete laboratories or government tenders — our export engineers prepare the configuration, proforma invoice and shipping documents.