Resin incoming inspection and lot certification run around the clock with a 20 to 50 position autosampler loading crimped or hermetic aluminium pans. A typical heat-cool-heat cycle takes 20–40 min, so an overnight queue clears a full day's samples. Range is −90 to 600 °C with heating up to 100 °C/min.

Autosampler capacity
20–50 positions
Temperature range
−90 to 600 °C with cooling
Heating rate
0.1–100 °C/min
Calorimetric accuracy
±1% (indium)
Temperature accuracy
±0.2 °C (indium)
Inquiry Now

Packing & Shipping

Place of originChina (dispatched from Shanghai)
BrandLiquid International / OEM on request
Export packingFumigation-free plywood case or reinforced carton
Loading portShanghai / Ningbo (others on request)
Payment termsT/T, L/C at sight (confirmed on quotation)
Trade termsEXW, FOB, CFR, CIF, DAP

Typical export terms — final terms are confirmed on the proforma invoice.

Product Description 产品描述

Resin incoming inspection and lot certification run around the clock with a 20 to 50 position autosampler loading crimped or hermetic aluminium pans. A typical heat-cool-heat cycle takes 20–40 min, so an overnight queue clears a full day's samples. Range is −90 to 600 °C with heating up to 100 °C/min.

Highlights

  • Unattended runs free technicians for sample preparation.
  • Compare each batch against a stored reference curve for grade identity.
  • Temperature accuracy of ±0.2 °C and calorimetric accuracy ±1%.
  • Suitable for checking recycled polymer sorting results.

Applications

  • Incoming inspection of resin batches
  • Grade identity verification against a reference curve
  • Production lot certification for thermoplastic compounds
  • Recycled polymer sorting verification

Specifications 技术参数

ParameterValue
Autosampler capacity 自动进样容量 20–50 positions
Temperature range 温度范围 −90 to 600 °C with cooling
Heating rate 升温速率 0.1–100 °C/min
Calorimetric accuracy 量热准确度 ±1% (indium)
Temperature accuracy 温度准确度 ±0.2 °C (indium)
Typical cycle time per sample 单样品典型周期 20–40 min for heat-cool-heat
Crucible types 坩埚类型 Crimped aluminium, hermetic aluminium
Purge gas flow 吹扫气流量 20–50 mL/min
Data output 数据输出 CSV, PDF report, network export
Power supply 电源 220 V, 50/60 Hz
Model No.DSCA-0004
Place of originChina (dispatched from Shanghai)

Applicable standards 适用标准

ISO 11357-1 ISO 11357-2 ISO 11357-3 ASTM D3418 ASTM E1356 ASTM D3895 IEC 61010-1

Chinese national standards (GB/T, JJG) and international standards referenced for this product type. Test reports and certificates are supplied with the quotation on request.

Packing & Shipping 包装与运输

Export packing

Fumigation-free plywood case or reinforced carton

Every unit is power-tested before packing; enclosed in shock foam and moisture barrier; wooden cases comply with ISPM 15.

Loading port

Shanghai / Ningbo (others on request)

Full container load (FCL), less-than-container load (LCL) or air freight; complete export documentation provided.

Inquiry Now 索取报价

Complete the form below — an export engineer will send technical configurations and a formal proforma invoice within 24 hours.

Products in this inquiry: Differential Scanning Calorimeter with Autosampler for Polymer QC (DSCA-0004)

We reply within 24 hours (Beijing Time, UTC+8). Your details are used only to answer this inquiry.

Related products

6 models

Send your equipment list — receive a formal quotation within 24 hours

Single instruments, complete laboratories or government tenders — our export engineers prepare the configuration, proforma invoice and shipping documents.