Moulders use this DSC to confirm polyolefin and polyamide grades, check crystallinity and verify melting after processing. It covers −90 to 600 °C with cooling, heats at up to 100 °C/min and achieves ±0.2 °C and ±1% accuracy on indium. Calibration uses indium, zinc and sapphire standards.

Temperature range
−90 to 600 °C with cooling accessory
Heating rate
0.1–100 °C/min
Temperature accuracy
±0.2 °C (indium)
Calorimetric accuracy
±1% (indium)
Crucible volume
40 µL standard, 100 µL optional
Inquiry Now

Packing & Shipping

Place of originChina (dispatched from Shanghai)
BrandLiquid International / OEM on request
Export packingFumigation-free plywood case or reinforced carton
Loading portShanghai / Ningbo (others on request)
Payment termsT/T, L/C at sight (confirmed on quotation)
Trade termsEXW, FOB, CFR, CIF, DAP

Typical export terms — final terms are confirmed on the proforma invoice.

Product Description 产品描述

Moulders use this DSC to confirm polyolefin and polyamide grades, check crystallinity and verify melting after processing. It covers −90 to 600 °C with cooling, heats at up to 100 °C/min and achieves ±0.2 °C and ±1% accuracy on indium. Calibration uses indium, zinc and sapphire standards.

Highlights

  • Measures OIT to confirm stabiliser levels.
  • Typical 5–10 mg samples in 40 µL crucibles.
  • 100 µL crucibles optional for bulky samples.
  • Purge flow from 20 to 50 mL/min.

Applications

  • Grade identity checks for polyolefins and polyamides
  • Crystallinity determination for moulding control
  • Melting point verification after processing
  • Oxidative induction time of stabilised grades

Specifications 技术参数

ParameterValue
Temperature range 温度范围 −90 to 600 °C with cooling accessory
Heating rate 升温速率 0.1–100 °C/min
Temperature accuracy 温度准确度 ±0.2 °C (indium)
Calorimetric accuracy 量热准确度 ±1% (indium)
Crucible volume 坩埚容积 40 µL standard, 100 µL optional
Purge gas flow 吹扫气流量 20–50 mL/min
Typical sample mass 典型样品量 5–10 mg
Calibration standards 校准标准物质 Indium, zinc, sapphire
Power supply 电源 220 V, 50/60 Hz
Model No.THA-0001
Place of originChina (dispatched from Shanghai)

Applicable standards 适用标准

ISO 11357-1 ISO 11358-1 ISO 11359-1 ISO 6721-1 ISO 306 ISO 75-1 ASTM D648 ASTM D1525 ASTM D4065 IEC 61010-1

Chinese national standards (GB/T, JJG) and international standards referenced for this product type. Test reports and certificates are supplied with the quotation on request.

Packing & Shipping 包装与运输

Export packing

Fumigation-free plywood case or reinforced carton

Every unit is power-tested before packing; enclosed in shock foam and moisture barrier; wooden cases comply with ISPM 15.

Loading port

Shanghai / Ningbo (others on request)

Full container load (FCL), less-than-container load (LCL) or air freight; complete export documentation provided.

Inquiry Now 索取报价

Complete the form below — an export engineer will send technical configurations and a formal proforma invoice within 24 hours.

Products in this inquiry: Differential Scanning Calorimeter for Plastics (THA-0001)

We reply within 24 hours (Beijing Time, UTC+8). Your details are used only to answer this inquiry.

Related products

6 models

Send your equipment list — receive a formal quotation within 24 hours

Single instruments, complete laboratories or government tenders — our export engineers prepare the configuration, proforma invoice and shipping documents.